(19)
(11)EP 3 116 976 B1

(12)EUROPEAN PATENT SPECIFICATION

(45)Mention of the grant of the patent:
04.11.2020 Bulletin 2020/45

(21)Application number: 15711623.7

(22)Date of filing:  11.03.2015
(51)International Patent Classification (IPC): 
C10B 1/04(2006.01)
F27D 1/10(2006.01)
C10B 55/00(2006.01)
F27D 1/14(2006.01)
(86)International application number:
PCT/US2015/019832
(87)International publication number:
WO 2015/138534 (17.09.2015 Gazette  2015/37)

(54)

INTERNAL LINING FOR DELAYED COKER DRUM

INNENAUSKLEIDUNG FÜR EINE DELAYED-COKER-TROMMEL

REVÊTEMENT INTERNE DE TAMBOUR D'UNITÉ DE COKÉFACTION DIFFÉRÉE


(84)Designated Contracting States:
AL AT BE BG CH CY CZ DE DK EE ES FI FR GB GR HR HU IE IS IT LI LT LU LV MC MK MT NL NO PL PT RO RS SE SI SK SM TR

(30)Priority: 12.03.2014 US 201461951614 P
13.05.2014 US 201461992316 P
09.03.2015 US 201514641903

(43)Date of publication of application:
18.01.2017 Bulletin 2017/03

(73)Proprietor: ExxonMobil Research and Engineering Company
Annandale, NJ 08801-0900 (US)

(72)Inventors:
  • HINSON, Christopher, S.
    Calgary, AB T3H 4N2 (CA)
  • FOWLER, Christopher, John
    Houston, TX 77095 (US)
  • SINCLAIR, David, Scott
    Houston, TX 77055 (US)
  • SUSONG, Adam, Garrett
    Spring, TX 77386 (US)
  • ANTRAM, Robert, Lee
    Warrenton, VA 20186 (US)
  • PETERSON, John, Roger
    Ashburn, VA 20147 (US)

(74)Representative: ExxonMobil Chemical Europe Inc. 
IP Law Europe Hermeslaan 2
1831 Machelen
1831 Machelen (BE)


(56)References cited: : 
US-A- 1 823 451
US-A1- 2008 003 125
US-A- 2 702 269
  
  • ANTALFFY L P ET AL: "INNOVATIONS IN DELAYED COKING COKE DRUM DESIGN", PROCEEDINGS OF THE JOINT ASME/JSME PRESSURE VESSELS AND PIPING, XX, XX, vol. 388, 1 August 1999 (1999-08-01), pages 207-217, XP008015222,
  • DEL PRETEA M ET AL: "Cladding of pressure equipment; case studies and the choice of various types of application. Case study: cladding in the fabrication of coke drums", WELDING INTERNATIONAL, TAYLOR & FRANCIS, ABINGDON, GB, [Online] vol. 28, no. 7/9, July 2014 (2014-07), pages 617-628, XP001588924, ISSN: 0950-7116, DOI: 10.1080/09507116.2012.753265 [retrieved on 2013-03-18]
  
Note: Within nine months from the publication of the mention of the grant of the European patent, any person may give notice to the European Patent Office of opposition to the European patent granted. Notice of opposition shall be filed in a written reasoned statement. It shall not be deemed to have been filed until the opposition fee has been paid. (Art. 99(1) European Patent Convention).


Description

Field of the Invention



[0001] This invention relates to a method of extending the fatigue life of delayed coking coke drums used for the thermal processing of heavy petroleum oils and more particularly, to the use of internal linings in delayed coking coke drums for extending their fatigue life.

Background of the Invention



[0002] Delayed coking is a process used in the petroleum refining industry for increasing the yield of liquid product from heavy residual oils such as vacuum resid.

[0003] In delayed coking, the heavy oil feed is heated in a furnace to a temperature at which thermal cracking is initiated but is low enough to reduce the extent of cracking in the furnace itself. The heated feed is then led into a large drum in which the cracking proceeds over an extended period of residence in the drum. The cracking produces hydrocarbons of lower molecular weight than the feed which, at the temperatures prevailing in the drum, are in vapor form and which rise to the top of the drum where they are led off to the downstream product recovery unit with its fractionation facilities. The thermal cracking of the feed that takes place in the drum also produces coke, which gradually accumulates in the drum during the delayed coking cycle. When the coke reaches a certain level in the drum, the introduction of the feed is terminated and the cracked products remaining in the drum are removed by purging with steam. After this, the coke is quenched with water, the drum is depressurized, the top and bottom heads are opened, and then the coke is discharged through the bottom head of the drum through use of a high pressure cutting water system. The cracking cycle is then ready to be repeated. Typically the process itself is achieved by heating the heavy oil feed to a temperature in the range that permits a pumpable condition in which it is fed into the furnace and heated to a temperature in the range of 380 to 525°C; the outlet temperature of a coker furnace is typically around 500°C with a pressure of 4 bar. The hot oil is then fed into the coke drum where the pressure is held at a low value in order to favor release of the vaporous cracking products, typically ranging from 1 to 6 bar, more usually around 2 to 3 bar. Large volumes of water are used in the quench portion of the coking cycle: one industry estimate is that for a typically large coke drum about 8m in diameter and 25m high, about 750 tonnes of water are required for quenching alone with even more required for the cutting operation after the drum is opened and the coke discharged. A useful and widely cited summary of the delayed coking process is available online in "Tutorial: Delayed Coking Fundamentals", Ellis et al, Great Lakes Carbon Corporation, Port Arthur, TX, AlChE 1998 Spring National Meeting, New Orleans, LA, 8-12 March 1998, Paper 29a, Copyright ©1998 Great Lakes Carbon Corporation.

[0004] Delayed coking coke drums are conventionally large vessels, typically at least 4 and possibly as much as 10m in diameter with heights of 10 to 30 m or even more. The drums are usually operated in twos or threes with each drum sequentially going through a charge-quench-discharge cycle, with the heated feed being switched to the drum in the feed phase of the cycle. The drums are typically made of unlined or clad steel, with base thicknesses that can range from about 10 to 30 mm thick. The internal cladding thickness is nominally 1-3 mm and is used for protection against sulfur corrosion. The present common commercial practice is to use 401S clad or unclad CS, C-1/2 Mo, or low chromium drums for delayed coking service. In form, the drums comprise vertical cylinders with either an ellipsoidal or hemispherical top head and a conical bottom head. The bottom head has either a flange or, alternatively, a mechanical valve arrangement as described, for example, in U.S. 6,843,889 (Lah). The feed inlet and steam/water connections are located in this lower conical section of the vessel. Operating envelopes and inspection/repair strategies are the mechanisms used to manage fatigue cracking in this equipment.

[0005] US 2,702,269 discloses a device for coking and cracking oils comprising a vertical cylindrical heating chamber having a downwardly tapering lower end part, and a thermally insulating cylindrical casing surrounding the heating chamber, the walls of the coking chamber being provided with a ceramic lining containing admixtures of heavy metal oxides in order to provide high heat transmission by radiation within the chamber. ANTALFFY L P ETAL: "INNOVATIONS IN DELAYED COKING COKE DRUM DESIGN", PROCEEDINGS OF THE JOINT ASME/JSME PRESSURE VESSELS AND PIPING, XX, XX, vol. 388, 1 August 1999 (1999-08-01), pages 207-217, discloses a coke drum construction method aimed at minimizing circumferential seals in order to avoid coke drum bulging and weld seam cracking. DEL PRETEA M ET AL: "Cladding of pressure equipment: case studies and the choice of various types of application. Case study; cladding in the fabrication of coke drums", WELDING INTERNATIONAL, TAYLOR & FRANCIS, ABINGDON, GB, vol. 28, no. 7/9, July 2014 (2014-07), pages 617-628, discloses a case study into cladding in the fabrication of coke drums, the cladding materials being austenic stainless steel, ferritic stainless steel, nickel alloys, copper alloys and titanium alloy.

[0006] Delayed Coker coke drums are inherently exposed to pressure boundary fatigue cracking due to the thermal stresses imposed on the steel primarily during the quench/fill process. The drums are prone to thermal fatigue due to the through-wall thermal stresses that are developed prior to the drum reaching steady state. Additionally, at the skirt-to-shell junction, the transient temperature differentials between the pressure boundary and the skirt also set up high stresses that can lead to weld and base metal cracking. This is a transient effect, and data analysis has shown that the other delayed coking steps (e.g., drum warm-up, feed introduction, coking, steam out, etc.) have less impact on pressure boundary stresses. As noted by Ellis, op. cit., the rate of cooling water injection is critical. Increasing the flow of water too rapidly can "case harden" the main channels up through the coker without cooling all of the coke radially across the coke bed. The coke has low porosity which then allows the water to flow away from the main channels in the coke drum, leading to the problem of drum bulging during cool down. If the rate of water is too high, the high pressure causes the water to flow up the outside of the coke bed cooling the wall of the coke drum. Coke has a higher coefficient of thermal expansion than does steel (154 for needle coke versus 120 for steel, cm/cm/°C x 10-7). While drum support systems such as that described in U.S. Patent No. 8,221,591 (de Para) may be capable of reducing the mechanical stresses generated by the differential cooling, it would nevertheless by desirable to minimize the transient thermal stress in both the coke drum shell/cone as well as at the skirt-to-shell junction.

Summary of the Invention



[0007] We now propose the use of a thermal buffering system to reduce or minimize the transient thermal stress that occurs in the steel during the portions of the coking cycle when the thermal stresses arise. The application of a lining system applied to the internal surface of the coke drum pressure boundary will be effective to reduce stresses on the drum during the operation of the process, particularly during the cooling/quench portion of the cycle. Coverage of the pressure boundary with internal lining can vary from a few meters of vessel height to all of the pressure boundary depending on (1) the level of protection needed in historically problematic areas (i.e., at the skirt-to-shell junction, in the bottom cone, near the outage level, etc.), and/or (2) to address efforts to minimize cycle time via shorter quench phases, feed introduction at lower drum warm-up temperatures, etc.

[0008] According to the present invention, the delayed coker coke drum has a monolithic, thermal shock-resistant, erosion-resistant refractory lining on the inner surface of the drum, especially in the areas subject to pressure boundary stress. The monolithic lining, applied by ramming in a similar manner to air-setting erosion-resistant refractory, is held in place by a suitable anchoring system, preferably a single point anchoring system as discussed further below. Anchoring systems of this type are customarily used for anchoring erosion-resistant refractory linings in petroleum processing vessels and may be used for the present purposes.

[0009] In an embodiment not according to the present invention, the delayed coker coke drum includes the same aforementioned anchoring system, but does not include the air setting erosion-resistant refractory. In this embodiment, the coke being fed into the coke drum fills the anchoring system and the two form an internal lining on the inner surface of the drum. This allows the transient thermal stress to be dissipated across a layer of coke rather than across the coke drum pressure boundary.

[0010] In another embodiment not according to the present invention, the delayed coker coke drum includes a pin and plate assembly. In this assembly, pins are provided extending inward from the outer wall of the coke drum. Attached to the pins are protective plates. The plates are arranged such that they create an air gap that will fill with a protective layer of coke between the coke being fed into the coke drum and the inner surface of the drum. This allows the transient thermal stress to be dissipated across the coke and the protective plates rather than across the coke drum pressure boundary. The protective plates prevent the removal of the protective coke layer during the cutting cycle.

Drawings



[0011] 

Figure 1 is a simplified vertical section of a delayed coker coke drum showing potential areas for the application of the internal lining.

Figure 2 illustrates an embodiment of the internal lining of the present invention.

Figure 3 illustrates an embodiment of the internal lining not according to the present invention.


Detailed Description



[0012] Figure 1 shows a section of a typical delayed coker coke drum 10 with its flanged vapor discharge outlet 11 on the hemispherical head at the top of the drum. The bottom conical head 13 terminates in the flanged bottom coke discharge outlet 14. The drum is supported on a skirt, as indicated at 15. The feed inlet is not shown but may conventionally be provided either in the bottom head that flanges up to the discharge outlet 14 or in the conical section 13. If the inlet is fixed in the cone, multiple feed inlets are preferred as described in US 7,736,470 (Chen); the feed inlets may be angled upwards as described in US 2013/0153466 (Axness).

[0013] Zones in the drum subject to pressure boundary stress are indicated in Fig. 1 as SZ1, SZ2, and SZ3. SZ1 indicates a typical weld area in the vertical cylindrical section of the drum where plates meet and cracking of the circumferential weld seams, base metal, and weld overlay/cladding is found. At SZ2 where the drum sits in the drum skirt (part of the drum support system welded to the drum around the lower periphery of the main cylindrical section), cracking of the skirt attachment weld and/or keyhole slots in the skirt is apt to be encountered. In the main cylindrical section of the drum at approximately SZ3, drum bulging may be encountered, with pressure boundary cracking at the bulge locations. In addition to circumferential weld, weld Heat-Affected Zone (HAZ), base metal, and internal cladding cracking, there have also been cases of cracking in the longitudinal weld seams and disbonding of the internal cladding.

[0014] According to the present invention, the delayed coker coke drum has a thermal shock-resistant lining applied to the inner surfaces of the drum. The lining has the function of reducing the thermally-induced mechanical stresses from the transient temperature cycles occurring during the delayed coking process, particularly common during the cooling/quench phase of the cycle, but present to a lesser extent during other phases. The lining is effective to minimize the transient thermal stress that occurs in the shell and bottom head and to reduce the high thermal stress resulting from temperature differentials at the skirt-to-shell junction.

[0015] Figure 2 shows an embodiment of the internal lining of the current invention. Anchoring system 22 is connected to the inner surface of pressure boundary 21. Anchoring system 22 forms the voids into which thermal barrier 23 can be inserted.

[0016] According to the invention, thermal barrier 23 is a refractory material. The cyclic service of the drum is such that a brick lining is unlikely to be satisfactory due to its inability to handle the thermal loads in the through-thickness direction. Additionally, a heat-resistant, monolithic refractory lining is also unlikely to handle such thermal cycling loads due to an inadequate anchorage system common for such refractory types. According to one embodiment of the invention the use of a thin-layer (3/4 - 2 inch (1.9 - 5 cm) nominally), thermally-shock resistant and erosion-resistant refractory lining is contained in appropriate anchorage that resists transient thermal loading.

[0017] Suitable refractories are those normally used for erosion-resistant linings in thermal processing units, such as those used in Fluid Catalytic Cracking Units (FCCUs), but with the essential qualifications that the erosion-resistant nature of the refractory also be thermal-shock resistant and capable of withstanding the cutting water pressure required to remove the coke from the drum as part of the normal decoking cycle. In all cases, the refractory should be selected to be as durable as possible. In view of the service requirements, three conceptual approaches are possible:
  • Use a high strength refractory material that is filled with a high level of a low expansion refractory aggregate. The effect of the rapid temperature changes encountered during the quench cycle is then minimized by the reduced dimensional change from thermal expansion. The material imparts a thermal barrier that delays the heat transfer to the base shell material.
  • Use a high strength refractory material that is filled with a high level of highly thermally conductive refractory aggregate. Rapid temperature changes are transmitted to the shell plate during the quench cycle. This minimizes the internal thermal stresses in the refractory material. The material imparts a minimal thermal barrier that more quickly transfers the heat to the base shell material yet provides adequate steel protection.
  • Use a high strength refractory material that is filled with a high level of an aggregate that closely matches the thermal expansion of the base plate. The impact of rapid temperature changes encountered during the quench cycle is then minimized by the reduced dimensional change from thermal expansion. The material imparts a thermal barrier that delays the heat transfer to the base shell material.


[0018] The specific refractory material used to implement these approaches may be selected on an empirical basis from the many castable refractories of this type that are commercially available. Selection of the specific refractories may be made according to experience in other petroleum refining applications, relations with suppliers, etc., as is normally the practice. Qualification of the lining should be established by transient thermal cycle tests (simulating actual delayed coker quench/ fill steps) to ensure optimized refractory/anchor system reliability.

[0019] An important feature of the drum linings is the anchoring system. Hexagonal mesh has been the preeminent thin layer lining system, typically available in standard thicknesses of ¾ inch (19 mm), 1inch (25 mm) and 2 inch (50 mm), although other thicknesses can be custom made. Hexagonal mesh is composed of long ribbons and the resultant lining system is comprised of discrete refractory cells bound by a metallic cell formed by the ribbons. Attachment of these long ribbons to the base material results in accumulation of thermal strain across the attachment welds (typically at 25 mm distances) resulting in failure. For this reason, hexagonal mesh is unlikely to be optimal as an anchoring system for service in the coke drum and will not be preferred. Experience in FCC units with hexmesh in coking service has shown that when the welds start to break, coke accumulates with each thermal cycle until all the welds break and the section falls off as a sheet. If used, hexagonal mesh should be installed in discrete sections that could pass through the outlet nozzle and not impede unloading if they became detached.

[0020] Alternatives to hexagonal mesh are single point anchoring systems in which thermal strain is accumulated only across the individual weld (3-10 mm diameter): stud weldable anchoring systems that minimize the potential for accumulated thermal strain across multiple attachment welds are preferred. The resultant systems provide a continuous refractory system with discrete anchoring points where the failure of a single anchor is less detrimental to the lining system than failure of a sheet secured by hexmesh. Individual I Anchors such as the Silicon CVC anchors, Hex-Alt anchors (e.g., K-bars™, Half Hex™, etc.), such as those shown, for instance, in US 6,393,789 (Lanclos), US D393588 (Tuthill), may be considered for potential use. An extensive range of refractory anchors is supplied commercially by the Hanlock-Causeway Company of Tulsa, OK and Houston, TX. Wear-resistant anchors such as Hanlock, Fiexmesh™, Tabs, hex cells, S-Anchor™ and stud gun weldable half hex cell anchors may also be useful. Typical anchoring systems are welded, usually by spot or stud welds to the underlying metal surface prior to application of the lining. Anchors should be welded directly to the surface (can be clad or unclad) of the coke drum, or alternatively, stud-welding technology may be employed for improved installation efficiency. These refractory anchors will typically extend directly out to the surface of the refractory lining. A description of refractory lining techniques including refractory materials and anchoring systems may be found in Refractories Handbook, Charles Schacht (Ed), CRC Press Content, August 2004, ISBN 9780824756543, to which reference is made for a description of refractory material, systems and application techniques such as may be used for forming the refractory linings in coke drums.

[0021] The refractory material will typically be installed by hand packing, ramming or hammering an air-setting refractory mix into place within the anchoring system attached to the shell wall of the drum. Refractory ramming mixes usually contain a plastic clay which is tempered with water (typically 2-5 percent). They are commonly supplied in a damp granular form ready for installation by hand packing or by using pneumatic rammers. The mix, containing refractory minerals and clay, can also include organic plasticizers to facilitate installation. Suitable mixes can be determined upon consultation with refractory suppliers as noted above when the specific site and service duties are fixed. Typical commercial ramming mixes include Rescobond AA-22S™, Actchem™ 75, Actchem™ 85, and the QNEX™ ramming products. As noted above, selection of the specific refractory material may be made on an empirical basis in light of the applicable service specifications.

[0022] Still referring to Figure 2, in an embodiment not according to the invention, thermal barrier 23 is the coke itself. During the coking cycle, coke will form in anchoring system 22 and will be present to insulate the drum during the quench/fill phase, forming thermal barrier 23. Although all or part of the coke will be removed via the high pressure cutting water process during the decoke phase, the coke will replenish itself in time for the next quench/fill cycle. In this embodiment, the coke performs the same function as the refractory described above.

[0023] Figure 3 shows yet another embodiment of the internal lining not according to the current invention. Anchoring pins 32 are connected to the inner surface of pressure boundary 31. Protective plates 34 are connected to the anchoring pins 32 so as to form an air gap. Said air gap will fill with coke creating an in situ thermal barrier 33. In this embodiment, the thermal stresses from the coking/decoking cycle are dissipated across protective plates 34 and thermal barrier 33, rather than across pressure boundary 31.

[0024] The present invention offers potential benefits in the following problem areas:
  1. 1. It minimizes and potentially mitigates thermal fatigue in coke drum shells caused by the transient thermal stress resulting from the quench/fill and heat-up steps of the decoking/coking cycle during the normal delayed coker operations. Finite Element Analyses have been performed to confirm the insulating effect of the refractory during these transient events and a reduction in thermal stress (at least one order of magnitude) in the underlying steel.
  2. 2. It minimizes or mitigates skirt-to-shell cracking by reducing the thermal stress caused by the transient temperature differential between the cone/shell of the coke drum and its skirt when coking and upon cool-down when decoking.
  3. 3. To fully capitalize on a reduced stress state at the skirt-to-shell junction, consideration may be given to positive benefits from selective external insulation removal in this area and design optimization of the skirt-to-shell junction.
  4. 4. Use of lining on the internal surface of the drum will allow operation with reduced decoking cycle time through reduced drum warm-up and/or quench/fill steps.
  5. 5. For those units that are drum-limited (i.e., where operating envelopes are established to minimize thermal stress in the drum}, there are significant incentives recognized through reduced cycle times.
  6. 6. Consideration may be given to removal of external insulation if the design proves effective in providing sufficient insulating characteristics to meet the needs of operations, resulting in potential cost savings and future inspection efficiency.
  7. 7. Use of internal lining on the internal surface of the coke drum may serve to eliminate the need for 410S internal cladding commonly used for protection against high temperature sulfidation with a consequential savings in unit capital costs. Removal of the 410S cladding from the initial design will also facilitate easier permanent repairs to the coke drums in the event that fatigue cracking does occur.
  8. 8. The properties of the refractory are likely to improve during use due to the strengthening effect offered by coke impregnation. Coke-impregnated refractory shows only slight reduction in thermal properties.
  9. 9. Embodiments with refractory lining have the potential to reduce or eliminate localized erosion incurred by the high pressure cutting water.



Claims

1. A delayed coking drum consisting of a top ellipsoidal or hemispherical head, a bottom conical head with an outlet for coke product, and a vertical cylindrical section, with a vapor outlet at the top and a feed inlet at/near the bottom, with a shock-resistant and erosion-resistant internal lining applied to the inner surface of the drum, wherein the internal lining is a refractory lining and wherein the refractory lining is a monolithic lining comprising a rammed refractory secured by means of anchors attached to the inner surface of the drum.
 
2. A delayed coking drum according to claim 1 in which the refractory lining is applied in the lower, conical section of the drum.
 
3. A delayed coking drum according to claim 1 in which the refractory lining is applied in the lower cylindrical section of the drum.
 
4. A delayed coking drum according to claim 1 in which the refractory lining is secured by means of a single point anchoring system attached to the inner surface of the drum, preferably in which the single point anchoring system is attached to the inner surface of the drum by means of stud welds in which thermal strain is accumulated only across individual welds.
 
5. A delayed coking drum according to claim 1 in which the thermally-shock resistant and erosion-resistant refractory lining has a thickness of 1.9 to 5 cm, or in which the thermally-shock resistant and erosion-resistant refractory lining comprises an air-setting rammed refractory.
 
6. A delayed coking process in which a heavy oil feed is heated in a furnace to a temperature at which thermal cracking is initiated, introducing the heated feed into a delayed coking coke drum having a top ellipsoidal or hemispherical head, a bottom conical head with an outlet for coke product, and a vertical cylindrical section, with a vapor outlet at the top and a feed inlet at/near the bottom, with a monolithic, shock-resistant and erosion-resistant refractory lining applied to the inner surface of the drum, wherein the refractory lining comprises a rammed refractory secured by means of anchors attached to the inner surface of the drum and coking the heated feed in the drum to produce thermally cracked hydrocarbon vapors and a coke product, purging cracked products remaining in the drum with steam, quenching the coke in the drum with water and discharging the quenched coke through the coke outlet.
 
7. A delayed coking process according to claim 6, in which the heavy oil feed is preheated to a temperature to bring the oil into a pumpable condition in which it is fed into the furnace.
 
8. A delayed coking process according to claim 7, in which the preheated heavy oil feed is heated in the furnace to a temperature in the range of 380 to 525°C.
 
9. A delayed coking process according to claim 6, in which the heavy oil feed is heated to promote coking in the coke drum at a pressure ranging from 1 to 6 bar.
 
10. A delayed coking process according to claim 6, in which the refractory lining comprises a rammed refractory secured by means of a single point anchoring system attached to the inner surface of the drum, preferably in which the single point anchoring system is attached to the inner surface of the drum by means of stud welds in which thermal strain is accumulated only across individual welds.
 
11. A delayed coking process according to claim 6, in which the thermally-shock resistant and erosion-resistant refractory lining has a thickness of 1.9 to 5 cm, or in which the thermally-shock resistant and erosion-resistant refractory lining comprises an air-setting rammed refractory, or in which the thermally-shock resistant and erosion-resistant refractory lining comprises discrete sections that are capable of passing through the coke product outlet.
 


Ansprüche

1. Delayed Coking-Trommel, die aus einem oberen ellipsoiden oder halbkugelförmigen Kopf, einem unteren konischen Kopf mit einem Auslass für Koksprodukt und einem vertikalen zylindrischen Abschnitt besteht, wobei sich im oberen Bereich ein Dämpfeauslass und am/nahe dem unteren Bereich ein Einsatzmaterialeinlass mit einer schockbeständigen und erosionsbeständigen Innenauskleidung befindet, wobei die Innenauskleidung eine hitzefeste Auskleidung ist, und wobei die hitzefeste Innenauskleidung eine monolithische Auskleidung ist, die ein gestampftes hitzefestes Material umfasst, das mittels Ankern an der Innenoberfläche der Trommel befestigt ist.
 
2. Delayed Coking-Trommel nach Anspruch 1, bei der die hitzefeste Auskleidung in dem unteren konischen Abschnitt der Trommel aufgebracht ist.
 
3. Delayed Coking-Trommel nach Anspruch 1, bei der die hitzefeste Auskleidung in dem unteren zylindrischen Abschnitt der Trommel aufgebracht ist.
 
4. Delayed Coking-Trommel nach Anspruch 1, bei der die hitzefeste Auskleidung mittels eines Einpunktverankerungssystems gesichert ist, welches an der Innenoberfläche der Trommel befestigt ist, wobei das Einpunktverankerungssystem vorzugsweise mittels Bolzenschweißstellen an der Innenoberfläche befestigt ist, bei denen thermische Spannung nur über individuellen Schweißstellen akkumuliert.
 
5. Delayed Coking-Trommel nach Anspruch 1, bei der die temperaturschockbeständige und erosionsbeständige hitzefeste Auskleidung eine Dicke von 1,9 bis 5 cm aufweist, oder bei der die temperaturschockbeständige und erosionsbeständige hitzefeste Auskleidung ein luftabbindendes gestampftes hitzebständiges Material aufweist.
 
6. Delayed Coking-Verfahren, bei dem ein Schweröleinsatzmaterial in einem Ofen auf eine Temperatur erhitzt wird, bei der thermisches Cracken initiiert wird, das erhitzte Einsatzmaterial in eine Delayed Coking-Kokstrommel mit einem oberen ellipsoiden oder halbkugelförmigen Kopf, einem unteren konischen Kopf mit einem Auslass für Koksprodukt und einem vertikalen zylindrischen Abschnitt eingebracht wird, wobei sich im oberen Bereich ein Dämpfeauslass und am/nahe dem unteren Bereich ein Einsatzmaterialeinlass befindet, wobei eine monolithische, schockbeständige und erosionsbeständige hitzefeste Auskleidung auf die Innenoberfläche der Trommel aufgebracht wird, wobei die hitzefeste Auskleidung ein gestampftes hitzefestes Material umfasst, das mittels Ankern gesichert ist, die an der Innenoberfläche der Trommel befestigt sind, und das erhitzte Einsatzmaterial in der Trommel verkokt wird, um thermisch gecrackte Kohlenwasserstoffdämpfe und ein Koksprodukt zu produzieren, gecrackte Produkte, die in der Trommel verbleiben, mit Wasserdampf ausgespült werden, der Koks in der Trommel mit Wasser gequencht wird und der gequenchte Koks durch den Koksauslass ausgetragen wird.
 
7. Delayed Coking-Verfahren nach Anspruch 6, bei dem das Schweröleinsatzmaterial auf eine Temperatur vorgeheizt wird, um das Öl in einen pumpbaren Zustand zu bringen, in dem es in den Ofen eingespeist wird.
 
8. Delayed Coking-Verfahren nach Anspruch 7, wobei das vorgeheizte Schweröleinsatzmaterial in dem Ofen auf eine Temperatur im Bereich von 380 bis 525°C erhitzt wird.
 
9. Delayed Coking-Verfahren nach Anspruch 6, bei dem das Schweröleinsatzmaterial erhitzt wird, um Verkoken in der Kokstrommel bei einem Druck im Bereich von 1 bis 6 bar zu fördern.
 
10. Delayed Coking-Verfahren nach Anspruch 6, bei dem die hitzefeste Auskleidung ein gestampftes hitzefestes Material umfasst, das mittels eines Einpunktverankerungssystems gesichert ist, welches an der Innenoberfläche der Trommel befestigt ist, wobei das Einpunktverankerungssystem vorzugsweise mittels Bolzenschweißstellen an der Innenoberfläche befestigt wird, bei denen thermische Spannung nur über individuellen Schweißstellen akkumuliert.
 
11. Delayed Coking-Verfahren nach Anspruch 6, bei dem die temperaturschockbeständige und erosionsbeständige hitzefeste Auskleidung eine Dicke von 1,9 bis 5 cm aufweist, oder bei dem die temperaturschockbeständige und erosionsbeständige hitzefeste Auskleidung ein luftabbindendes gestampftes hitzefestes Material umfasst, oder bei dem die temperaturschockbeständige und erosionsbeständige hitzefeste Auskleidung diskrete Abschnitte umfasst, die in der Lage sind, den Koksproduktauslass zu passieren.
 


Revendications

1. Tambour de cokéfaction différée consistant en une tête supérieure ellipsoïdale ou hémisphérique, une tête de fond conique munie d'une sortie pour un produit coke, et une section cylindrique verticale, avec une sortie de vapeur en haut et une entrée d'alimentation au niveau/à proximité du fond, avec un revêtement interne résistant aux chocs et résistant à l'érosion appliqué sur la surface interne du tambour, le revêtement interne étant un revêtement réfractaire et le revêtement réfractaire étant un revêtement monolithique comprenant un réfractaire damé fixé au moyen d'ancrages attachés à la surface interne du tambour.
 
2. Tambour de cokéfaction différée selon la revendication 1 dans lequel le revêtement réfractaire est appliqué dans la section conique inférieure du tambour.
 
3. Tambour de cokéfaction différée selon la revendication 1 dans lequel le revêtement réfractaire est appliqué dans la section cylindrique inférieure du tambour.
 
4. Tambour de cokéfaction différée selon la revendication 1 dans lequel le revêtement réfractaire est fixé au moyen d'un système d'ancrage à point unique attaché à la surface interne du tambour, de préférence dans lequel le système d'ancrage à point unique est attaché à la surface interne du tambour au moyen de soudures de goujons dans lesquelles la contrainte thermique est accumulée uniquement au travers de soudures individuelles.
 
5. Tambour de cokéfaction différée selon la revendication 1 dans lequel le revêtement réfractaire résistant aux chocs thermiques et résistant à l'érosion a une épaisseur de 1,9 à 5 cm, ou dans lequel le revêtement réfractaire résistant aux chocs thermiques et résistant à l'érosion comprend un réfractaire damé durcissant à l'air.
 
6. Procédé de cokéfaction différée dans lequel une alimentation d'huile lourde est chauffée dans un fourneau à une température à laquelle un craquage thermique est initié, l'alimentation chauffée est introduite dans un tambour de cokéfaction différée ayant une tête supérieure ellipsoïdale ou hémisphérique, une tête de fond conique munie d'une sortie pour un produit coke, et une section cylindrique verticale, avec une sortie de vapeur en haut et une entrée d'alimentation au niveau/à proximité du fond, avec un revêtement réfractaire monolithique résistant aux chocs et résistant à l'érosion appliqué sur la surface interne du tambour, le revêtement réfractaire comprenant un réfractaire damé fixé au moyen d'ancrages attachés à la surface interne du tambour, et l'alimentation chauffée est cokéfiée dans le tambour afin de produire des vapeurs hydrocarbonées craquées thermiquement et un produit coke, les produits craqués restant dans le tambour sont purgés avec de la vapeur, le coke est trempé dans le tambour avec de l'eau, et le coke trempé est déchargé par la sortie de coke.
 
7. Procédé de cokéfaction différée selon la revendication 6, dans lequel l'alimentation d'huile lourde est préchauffée à une température afin de mettre l'huile dans un état pompable dans lequel elle est introduite dans le fourneau.
 
8. Procédé de cokéfaction différée selon la revendication 7, dans lequel l'alimentation d'huile lourde préchauffée est chauffée dans le fourneau à une température dans la plage allant de 380 à 525 °C.
 
9. Procédé de cokéfaction différée selon la revendication 6, dans lequel l'alimentation d'huile lourde est chauffée pour favoriser la cokéfaction dans le tambour de cokéfaction à une pression allant de 1 à 6 bar.
 
10. Procédé de cokéfaction différée selon la revendication 6, dans lequel le revêtement réfractaire comprend un réfractaire damé fixé au moyen d'un système d'ancrage à point unique attaché à la surface interne du tambour, de préférence dans lequel le système d'ancrage à point unique est attaché à la surface interne du tambour au moyen de soudures de goujons dans lesquelles la contrainte thermique est accumulée uniquement au travers de soudures individuelles.
 
11. Procédé de cokéfaction différée selon la revendication 6, dans lequel le revêtement réfractaire résistant aux chocs thermiques et résistant à l'érosion a une épaisseur de 1,9 à 5 cm, ou dans lequel le revêtement réfractaire résistant aux chocs thermiques et résistant à l'érosion comprend un réfractaire damé durcissant à l'air, ou dans lequel le revêtement réfractaire résistant aux chocs thermiques et résistant à l'érosion comprend des sections discrètes qui sont capables de passer au travers de la sortie de produit coke.
 




Drawing














Cited references

REFERENCES CITED IN THE DESCRIPTION



This list of references cited by the applicant is for the reader's convenience only. It does not form part of the European patent document. Even though great care has been taken in compiling the references, errors or omissions cannot be excluded and the EPO disclaims all liability in this regard.

Patent documents cited in the description




Non-patent literature cited in the description