(19)
(11) EP 1 507 090 A8

(12) CORRECTED EUROPEAN PATENT APPLICATION
published in accordance with Art. 158(3) EPC

(48) Corrigendum issued on:
11.05.2005 Bulletin 2005/19

(43) Date of publication:
16.02.2005 Bulletin 2005/07

(21) Application number: 03728107.8

(22) Date of filing: 19.05.2003
(51) International Patent Classification (IPC)7F16C 33/32, C21D 1/18, C22C 38/00, B60B 35/14
(86) International application number:
PCT/JP2003/006237
(87) International publication number:
WO 2003/100277 (04.12.2003 Gazette 2003/49)
(84) Designated Contracting States:
AT BE BG CH CY CZ DE DK EE ES FI FR GB GR HU IE IT LI LU MC NL PT RO SE SI SK TR
Designated Extension States:
AL LT LV MK

(30) Priority: 23.05.2002 JP 2002149428

(71) Applicant: NTN CORPORATION
Osaka-shi Osaka 550-0003 (JP)

(72) Inventors:
  • MATSUBARA, Yukio, c/o NTN Corporation
    Kuwana-shi, Mie 511-0811 (JP)
  • MAEDA, Kikuo, c/o NTN Corporation
    Kuwana-shi, Mie 511-0811 (JP)

(74) Representative: GROSSE BOCKHORNI SCHUMACHER 
Patent- und Rechtsanwälte Forstenrieder Allee 59
81476 München
81476 München (DE)

   


(54) ROLLING PART AND POWER TRANSMISSION PART


(57) There is provided a rolling component formed of a steel material of the medium carbon steel level that provides a rolling life improved to be comparable to that of bearing steel and also provides improved characteristic against surface-cracking, and a power transmission component including the rolling component. To achieve this, the rolling component is formed of steel having an induction hardened portion having a stress intensity factor range associated with tension associated-fatigue crack extension that has a lower limit ΔKth of 6.2 Mpa√m.