(19) |
 |
|
(11) |
EP 4 345 980 A8 |
(12) |
CORRECTED EUROPEAN PATENT APPLICATION |
|
Note: Bibliography reflects the latest situation |
(15) |
Correction information: |
|
Corrected version no 1 (W1 A1) |
(48) |
Corrigendum issued on: |
|
08.05.2024 Bulletin 2024/19 |
(43) |
Date of publication: |
|
03.04.2024 Bulletin 2024/14 |
(22) |
Date of filing: 20.12.2022 |
|
(51) |
International Patent Classification (IPC):
|
(52) |
Cooperative Patent Classification (CPC): |
|
H01M 10/54 |
|
(84) |
Designated Contracting States: |
|
AL AT BE BG CH CY CZ DE DK EE ES FI FR GB GR HR HU IE IS IT LI LT LU LV MC ME MK MT
NL NO PL PT RO RS SE SI SK SM TR |
|
Designated Extension States: |
|
BA |
|
Designated Validation States: |
|
KH MA MD TN |
(30) |
Priority: |
30.09.2022 US 202217957753
|
(71) |
Applicant: Ascend Elements, Inc. |
|
Westborough, MA 01581 (US) |
|
(72) |
Inventors: |
|
- Kim, Kee-Chan
Westborough, 01581 (US)
- Matthew, Eggert
Westborough, 01581 (US)
|
(74) |
Representative: Greaves Brewster LLP |
|
Copa House
Station Road Cheddar, Somerset BS27 3AH Cheddar, Somerset BS27 3AH (GB) |
|
|
|
(54) |
NICKEL-METAL HYDRIDE (NIMH) BATTERY RECYCLING |
(57) Recycling of nickel-metal hydride (NiMH) batteries extracts substantially pure nickel
based on adding a leach agent to granular cathode material resulting from agitation
of the NiMH batteries to form a leach solution. A pH of the leach solution is maintained
for precipitating iron, aluminum and lanthanide rare earth elements (REE) for yielding
a nickel solution for forming a cathode material precursor in a recycled battery,
often with a high nickel content.